Emission of Volatile Oganic Compounds from Wood and Wood-Based Materials |
|
|||
Table. |
Result sensory testing |
Spruce |
Beech veneered particleboard with PVA-glue |
UV-curing lacquer on beech veneered particleboard |
|||
Acceptability |
Intensity |
Acceptability |
Intensity |
Acceptability |
Intensity |
|
Specimen Median |
0.5 |
1.3 |
0.3 |
1.7 |
0.7 |
1.0 |
Specimen Average |
0.5 |
1.2 |
0.3 |
1.7 |
0.5 |
1.4 |
Reference Median |
0.9 |
0.2 |
0.9 |
0.2 |
1.0 |
0.2 |
Reference Average |
0.9 |
0.3 |
0.8 |
0.4 |
0.9 |
0.3 |